4 PrincipleA pipe of specified length is placed in a liquid bath or air oven at a specified temperature for a specified time .A marked length of this portion of pipe is measured, under identical conditions, before and after heating. The reversion is calculated as a percentage of the change in length in relation to … Continue reading ISO 2505 – Thermoplastics Pipes — Longitudinal Reversion — Test Method and Parameters – Testing Equipment